pic 1 is the square in a box from a local auction
pic 2 is the ice cream tub of molasses it spent a month or so in there, scrubbed it with a scotchbrite kitchen scrub pad
pic 3 in the quicky phosphoric acid container for just the square about 20-30 minutes in that, it is a weak solution is like a painter product called metal prep, this happens to be diluted etch & prep by Kwik-kleen
pic 4 is one side after the metal prep, as it dries. the metal prep keeps the metal from flash rusting after being in the molasses